observed along with well-developed dimples in alloys having relatively 
uniform carbide dispersions, such as HY-130 steel, and because TTS is observed under varying stress states. A detailed 
discussion of the TTS fracture mode is available in Ref 91. 
 
References cited in this section 
1. I. Le May, Metallography in Failure Analysis, J.L. McCall and P.M. French, Ed., American Society for 
Metals, 1977 
2. F.P. McClintock and G.R. Irwin, in Fracture Toughness Testing and Its Applications, STP 381, American 
Society for Testing and Materials, 1965, p 84-113 
3. P.C. Paris and G.C. Sih, in Fracture Toughness Testing and Its Applications, STP 381, American Society 
for Testing and Materials, 1965, p 30-81 
4. B.V. Whiteson, A. Phillips, V. Kerlins, and R.A. Rawe, Ed., in Electron Fractography, STP 436, American 
Society for Testing and Materials, 1968, P 151-178 
5. C.D. Beachem, Metall. Trans. A, Vol 6A, 1975, p 377-383 
6. C.D. Beachem and D.A. Meyn, in Electron Fractography, STP 436, American Society for Testing and 
Materials, 1968, p 59 
7. J. Friedel, in Fracture, Proceedings of the Swampscott Conference, MIT Press, 1959, p 498 
8. C.D. Beachem, Liebowitz Fracture I, Academic Press, 1968, p 243-349 
9. H. Schardin, in Fracture, Proceedings of the Swampscott Conference, MIT Press, 1959, p 297 
10. J.P.E. Forsyth, Acta Metall., Vol 11, July 1963, p 703 
11. C. Laird and G.C. Smith, Philos. Mag., Vol 7, 1962, p 847 
12. W.A. Wood and A.K. Head, J. Inst. Met., Vol 79, 1950, p 89 
13. W.A. Wood, in Fracture, Proceedings of the Swampscott Conference, MIT Press, 1959, p 412 
14. C.V. Cooper and M.E. Fine, Metall. Trans. A, Vol 16A (No. 4), 1985, p 641-649 
15. R.O. Ritchie, in Environment-Sensitive Fracture of Engineering Materials, Z.A. Foroulis, Ed., The 
Metallurgical Society, 1979, p 538-564 
16. O. Buck, W.L. Morris, and M.R. James, Fracture and Failure: Analyses, Mechanisms and Applications, 
P.P. Tung, S.P. Agrawal, A. Kumar, and M. Katcher, Ed., Proceedings of the ASM Fracture and Failure 
Sessions at the 1980 Western Metal and Tool Exposition and Conference, Los Angeles, CA, American 
Society for Metals, 1981 
17. C.E. Richards and T.C. Lindley, Eng. Fract. Mech., Vol 4, 1972, p 951 
18. R.O. Ritchie and J.F. Knott, Mater. Sci. Eng., Vol 14, 1974, p 7 
19. R.M.N. Pelloux, Trans. ASM, Vol 62, 1969, p 281-285 
20. D. Broek and G.O. Bowles, Int. J. Fract. Mech., Vol 6, 1970, p 321-322 
21. P. Neumann, Acta Metall., Vol 22, 1974, p 1155-1178 
22. R.M.N. Pelloux, in Fracture, Chapman and Hall, 1969, p 731 
23. R. Koterazawa, M. Mori, T. Matsni, and D. Shimo, J. Eng. Mater. Technol., (Trans. ASME), Vol 95 (No. 
4), 1973, p 202 
24. F.E. Fujita, Acta Metall., Vol 6, 1958, p 543 
25. D.A. Meyn, Trans. ASM, Vol 61 (No. 1), 1968, p 42 
26. D.L. Davidson and J. Lankford, Metall. Trans. A, Vol 15A, 1984, p 1931-1940 
27. R.D. Carter, E.W. Lee, E.A. Starke, Jr., and C.J. Beevers, Metall. Trans. A, Vol 15A, 1984, p 555-563 
28. J.C. McMillan and R.M.N. Pelloux, Eng. Fract. Mech., Vol 2, 1970, p 81-84 
29. C.D. Beachem, Trans. ASM, Vol 60 (No. 3), 1967, p 325 
30. R.W. Hertzberg, Fatigue Fracture Surface Appearance, in Fatigue Crack Propagation, STP 415, American 
Society for Testing and Material, 1967, p 205 
31. P.C. Paris and F. Erdogan, J. Basic Eng., (Trans. ASME), D, Vol 85, 1963, p 528 
32. H.H. Johnson and P.C. Paris, Eng. Fract. Mech., Vol 1, 1968, p 3 
33. R.M.N. Pelloux, Trans. ASM, Vol 57, 1964, p 511 
34. D. Broek, in Fracture, Chapman and Hall, 1969, p 754 
35. D. Broek, Report NLR TR 72029U (AD-917038), National Aerospace Laboratory, 1972 
36. A.R. Troiano, Trans. ASM, Vol 52, 1960, p 54 
37. N.J. Petch, Philos. Mag., Vol 1, 1956, p 331 
38. C.D. Beachem, Metall. Trans. A, Vol 3A, 1972, p 437 
39. J.A. Clum, Scr. Metall., Vol 9, 1975, p 51 
40. C.A. Zapffe and C.E. Sims, Trans. AIME, Vol 145, 1941, p 225 
41. A.J. Forty, Physical Metallurgy of Stress Corrosion Cracking, Interscience, 1959, p 99 
42. H.L. Logan, J. Res. Natl. Bur. Stand., Vol 48, 1952, p 99 
43. T.P. Hoar and J.G. Hines, Stress Corrosion Cracking and Embrittlement, John Wiley & Sons, 1956, p 107 
44. I. Yamauchi and F. Weinberg, Metall. Trans. A, Vol 14A, 1983, p 939-946 
45. K.E. Puttick, Philos. Mag., Vol 4, 1959, p 964-969 
46. F.A. McClintock, J. Appl. Mech. (Trans. ASME), Vol 35, 1968, p 363-371 
47. A.S. Argon, J. Im, and R. Safoglu, Metall. Trans. A, Vol 6A, 1975, p 825-837 
48. M.F. Ashby, C. Gandhi, and D.M.R. Taplin, Acta Metall., Vol 27, 1979, p 699-729 
49. T. Veerasooriya and J.P. Strizak, Report ONRL/TM-7255, Oak Ridge National Laboratory, 1980 
50. I. Servi and N.J. Grant, Trans. AIME, Vol 191, 1951, p 909-922 
51. J.N. Greenwood, D.R. Miller, and J.W. Suiter, Acta Metall., Vol 2, 1954, p 250-258 
52. R.W. Baluffi and L.L. Seigle, Acta Metall., Vol 3, 1965, p 170-177 
53. A.J. Perry, J. Mater. Sci., Vol 9, 1974, p 1016-1039 
54. D.A. Miller and R. Pilkington, Metall. Trans. A, Vol 9A, 1978, p 489-494 
55. R. Raj and M.F. Ashby, Acta Metall., Vol 23, 1975, p 653-666 
56. J.A. Williams, Acta Metall., Vol 15, 1967, p 1119-1124, 1559-1562 
57. C.C. Law and M.J. Blackburn, Metall. Trans. A, Vol 11A (No. 3), 1980, p 495-507 
58. D.S. Wilkinson, K. Abiko, N. Thyagarajan, and D.P. Pope, Metall. Trans. A, Vol 11A (No. 11), 1980, p 
1827-1836 
59. K. Sadananda and P. Shahinian, Met. Sci. J., Vol 15, 1981, p 425-432 
60. J.L. Bassani, Creep and Fracture of Engineering Materials and Structures, B. Wilshire and D.R. Owen, 
Ed., Pineridge Press, 1981, p 329-344 
61. T. Watanabe, Metall. Trans. A, Vol 14A (No. 4), 1983, p 531-545 
62. I-Wei Chen, Metall. Trans. A, Vol 14A (No. 11), 1983, p 2289-2293 
63. M.H. Yoo and H. Trinkaus, Metall. Trans. A, Vol 14A (No. 4), 1983, p 547-561 
64. S.H. Goods and L.M. Brown, Acta Metall., Vol 27, 1979, p 1-15 
65. D. Hull and D.E. Rimmer, Philos. Mag., Vol 4, 1959, p 673-687 
66. R. Raj, H.M. Shih, and H.H. Johnson, Scr. Metall., Vol 11, 1977, p 839-842 
67. R.L. Coble, J. Appl. Phys., Vol 34, 1963, p 1679 
68. F.C. Monkman and N.J. Grant, Proc. ASTM, Vol 56, 1956, p 593-605 
69. R. Raj, Acta Metall., Vol 26, 1978, p 341-349 
70. A.N. Stroh, Adv. Phys., Vol 6, 1957, p 418 
71. J.O. Stiegler, K. Farrell, B.T.M. Loh, and H.E. McCoy, Trans. ASM, Vol 60, 1967, p 494-503 
72. I-Wei Chen and A.S. Argon, Acta Metall., Vol 29, 1981, p 1321-1333 
73. D.A. Miller and T.G. Langdon, Metall. Trans. A, Vol 10A (No. 11), 1979, p 1635-1641 
74. K. Sadananda and P. Shahinian, Metall. Trans. A, Vol 14A (No.7), 1983, p 1467-1480 
75. C.D. Beachem, B.F. Brown, and A.J. Edwards, Memorandum Report 1432, Naval Research Laboratory, 
1963 
76. T. Inoue, S. Matsuda, Y. Okamura, and K. Aoki, Trans. Jpn. Inst. Met., Vol 11, 1970, p 36 
77. I.M. Bernstein, Metall. Trans. A, Vol 1A, 1970, p 3143 
78. C.D. Beachem, Metall. Trans. A, Vol 4A, 1973, p 1999 
79. Y. Kikuta, T. Araki, and T. Kuroda, in Fractography in Failure Analysis, STP 645, B.M. Strauss and W.M. 
Cullen, Jr., Ed., American Society for Testing and Materials, 1978, p 107 
80. F. Nakasoto and I.M. Bernstein, Metall. Trans, A, Vol 9A, 1978, p 1317 
81. Y. Kikuta and T. Araki, in Hydrogen Effects in Metals, I.M. Bernstein and A.W. Thompson, Ed., The 
Metallurgical Society, 1981, p 309 
82. Y.H. Kim and J.W. Morris, Jr., Metall. Trans. A, Vol 14A, 1983, p 1883-1888 
83. A.R. Rosenfield, D.K. Shetty, and A.J. Skidmore, Metall. Trans. A, Vol 14A, 1983, p 1934-1937 
84. R.O. Ritchie, F.A. McClintock, H. Nayeb-Hashemi, and M.A. Ritter, Metall. Trans. A, Vol 13A, 1982, p 
101 
85. I. Aitchison and B. Cox, Corrosion, Vol 28, 1972, p 83 
86. J. Spurrier and J.C. Scully, Corrosion, Vol 28, 1972, p 453 
87. D.B. Knorr and R.M. Pelloux, Metall. Trans. A, Vol 13A, 1975, p 73 
88. R.J.H. Wanhill, Corrosion, Vol 32, 1976, p 163 
89. D.A. Meyn and E.J. Brooks, in Fractography and Material Science, STP 733, L.N. Gilbertson